Tape creep Testing Machine

The adhesive strength of the tape is assessed within a specified temperature range (40°C – 80°C), with the capability to analyze up to 12 samples simultaneously. Moreover, upon request, tapes can be custom-manufactured to withstand temperatures of up to 200°C.

Main specifications

Load

0.1〜2kg

Temperature

40〜80℃

Size

1900×800×1550mm

Power supply

AC200V 30A